1. Adair PJ, Oross-mann DG. The castable ceramic crown. Int J Periodom and Rcstor Dent 1984; 2: 33-4.^.
2.
Akı
n H, Seramik Diş hekimliğinde porselen. 2. Baskı. İÜ Diş Hck- Fak, İstanbul, 1983; i -34.
3.
Alkumrt
ı HN, Kedici S. Porselen jaket kron vapurunda yeni bir materyal vc teknik: Hi-Cerarru Oral 1988; 5: 52-53-54,20-24.
4. Anderson M, Odcn A- A new all ceramic crown. Acta Odontol Scatıd 1993; 51, 59-64.
5. Aııusavice KJ, Hjjatic B. tensile stress in ^lass ceramic crowns: Effect of flaws and cement voids, Int J
1-. . f |-|IV^ . c.i 1; -> ICO
riUÜLll -J.Ji-JJü.
6. Beham G. IPS Empress: A new ceramic technology. Ivoclar-Vivadent Report Nr. 6 September, 1990:3-15¬7 Beham G. IPS Hmpress: F.iııe nene
kcrainik-technologicZWR. lOO.Jahrg 1991:404-408.
H. Hienick KW, Marx R. Die mechanischc belaslbarkeit neaer vollkcramischer kronen und briickcnmaterialen. Sen Monat Zahnmeil 1994; 104: 3,
284-289,
9. Burke FJT, Quallrongh AJE, Male RW. The dentine-bonded ceramic crown: an ideal restoration. British Dent J 1995; 179: 2: ,58-63.
10. Champbell SD. Sozio RB. Evaluation of the fil and straight of an all-ceramic fixed partial denilire. J Proslhet Dent 1988; 59:3, 301-306
13. Champbell SD. Bslhetic modification of cast dental ceramic restorations. Int .1 Prosth 1990; 3:2, 123-129.
12. Chan C, HaraszLhy G, Geis-Gerstorfer J, Weber I [. The marginal tit of Ccrcslare hill ceramic crowns a preliminary report. Quint Int 1985: 6, 399-402.
13.
Çırhadaroğl
u f Melal destekli seramik kronlar. Kırın köprü protezi. 2. Baski AU. Diş. Hek. Fak., Ankara. 1977: Bölüm II, 125-190.
14. Dong .IK, Luthy Hn Wohlewend A, Schörer P. ] leal Pressed Ceramics; Techonolagy and strcnghL. Int .1 Prosth 1992; 5: 1,90-16
35. Donovan T. Prince J. An analysis ol margin configurations for metal ceramic crowns. J l^rosthet Dcni 1985:53:2, 153-157,
85
Atatürk Üniv.Dis, Hck.Fak.Dcrg. Cilt: 10, Sayı:2, Sayla:79-88, 2000
YÜKSEL .ÇEKİÇ, ÖZKAN
16. Felton DA, Kanoy BE, Bayııe SC, Wirthman GF. Hileci of in vivn crown margin discrepancies on periodontal health. J Prosthet Dent 1991; 65(3): 357-364.
17. Garber DA. Goldstein RK. Cast ceramic-systems and other alternatives. Quint. Pub. inc. Co, Uinois, 1995: 104-115.
18. Grey NJA, Piddock V, Wilson MA. In vitro comparison of conventional crowns and a new all ceramic system. J Dent Res 1993:21:47-51.
19. Grossman DG. Cast glass ceramics. Dent Clin North Am 1985; 29(4): 725-739.
20 Heinzmann İL, Krejci I. Lal/. F. Wear and marginal adaptation oi' glass ceramic inlays, amalgam and enamel. J Dent Res, 1990: 69; 161: Abstr. Nr:423.
21. Hübu S, Fvala T. Castable apatite ceramics aç a new biocompatible restorative material. I. Theoretical considerations. Quint Int. 19S5;2: 135-141.
22. Hobo S, Iwata T. Castable apatite ceramics as a new biocompatible restorative material. II, Fabrication of the restoration. Quint Int, 1985; 3: 207-216.
23. Hobo S, Iwata T. A new laminate veneer technique using a caslablc apaLilc ceramic material. II Practical procedures. Quint Int 1985; S: 509-517.
24. Hobo S, Iwata T_ A new laminate veneer technique using a castable apatite ceramic material I. Theoretical considerations. Quint Int 1 985; 7: 45 İ-458.
25. Holand W, Frank M. Material science of empress glass ceramics. Ivoclar Vivadent Report. No. 10, 1994: July 3-8.
26. Hondrum SO- The strength of alumina and magnesia core crowns. Int J Prosth 1988; 1(1): 67-72.
27. Hondrum SO. A review of the strength properties of dental ceramics J Prosthet Deni 1992; 67(6): 859-865.
28. Jcndcrscn MD, Allen EP, Bayne SC, Donovan TE. Hansson TL. Klooster J, Preston JD. Annual review of Selected dental literature: Report of the Committee on Scientific Investigation of the American Academy of Restorative Dentistry. .1 Prosthet Dent 1993: 70(1): 44-85.
29. Jûsephson BA, Şchnlmaıı A. Dunn ZA, HuAVİtz W. A Compressive strength study of an all ceramic crown. J Prosthet Dent 1985; 53(3): 301-303.
30.
Kedic
i S. Diş hekimliğinde apatit seramik teknolojisi. MÜ Diş Hck. Fak. Dcrg 1985:9(3-4): 261-269
31.
Kedic
i S. Metal desteksin seramik restorasyonlar. TDBÜ, 1994; 24: 22-23.
32. Kelsey WP, Cavel WT, Blankenau RJ, Barkmcicr WW, Wilwerding "I'M, Malıaııga I.F. Two year clinical study of eastable ceramic crowns. Quint Int 1995: 26(1): 15-20.
33. Krejci 1, Krejci D, Lutz F. Clinical evaluation of a new pressed glass ceramic inlay material over 1,5 years. Quint Int. İ992; 23(3): ISM 86.
34. Fang SA, Starr CB. Castable glass ceramics for veneer restorations. J Prosthet Dent 1992; 67(5): 590-594.
3.5. I_ehner C, Studer Scharer P. Full porcelain crowns made by IPS Empress first clinical results. .1 Dent Res, 1992; 71: 658, 1-3.
36- Levy If Working with the In-Ccram Porcelain System. Prolhese Dem 1990; 44(45): 1-11.
37. Ludwing K. Studies on the ultimate slrenglh of all -ceramic crowns. Dental - Labor. 1991:39: 647-651.
38. Liıthy H, Dong JK. WohJwend A, Scharer P. Heat pressed ceramics: Influence oi" veneering and gla7İng on strength..1 Dent Res, E992; 72: 567: Abstr. Nr: 415.
39. Liıthy H, Dong JK, Wohlwend A, Scharer P. Hileci ol" veneering and glaring on the slrcnght of heat pressed ceramics. Schweiz Monalsscbr Zahnmed, 1993;
103: 1257-1260.
40 Malament KA, Grossman DG. The cast glass ceramic restoration. J Prosthet Dent 1987; 57( 6t: 674-6K2.
41. Manic FK, Brantley WA, Dhulu VD,Zıcbert G.I. Fracture toughness of high alumina core dental ceramics: "the effect of water and artificial saliva. Int J Prosth 1993; 6(6): 546-552.
42. Maruyama T, Koh N, Hina T, Miyauehi S. Clinical use of a new castable glass ceramic material. Int .1 Prosth 1991; 4(2): 138-146.
43. McLean JW. The science and art of dental ceramics. Vol 1: The nature of dental ceramics and their clinical use. Quintcs. Pub. Co. Inc., IlIİtîois, 1979: 19-21.
44. Mclean JW. Kcdge MI. High strength ceramics. Quint Jut 1987; 18:2, 97^ 106.
45. Mc Lean JW. The science and art of denial ceramics. Operat Dent 1991; 16: 149-156.
86
Atatürk Üntv.DişHck.Fak.Derg. Cilt: İÜ, Sayı:2, Sayfa: 79-88, 2000
YÜKSFL,ÇEKİÇ, ÖZKAN
46. MolTa .İP, Lugassy AA, Ellison JA. Clinical evaluation of a castable ceramic material. J Dent Res 1988; 67, Abst. No: 43,118.
47. MUJIO/ CA, Goodacre CJ, Moore BK, Dykema RW. A comparative study of the strenght of aluminous porcelain jacket crowns constructed with the conventional and twin foil technique. J PcusLhet Dent 1982: 48(3): 271-281.
48. Myers ME. Ergle JW, Fuirhurst CW, Ringle liD. h'atiqiie failure parameters of IPS Empress porcelain. Int J Prosth. 1994; 7( 6): .549-553.
49. Nahara Y, Sadatnorı S, Hamada T. Clinical evaluation ot" castable apatite ceramic crowns. J Prosthet Dent 1991, 66(6): 754-758.
50. Maylor WP, Munoz CA, Goodacrc CJ. Swarts ML, Moore BK. The effect of surface treatment on the knoop hardness of Dieor. Int J Prosth 1991; 4(2): 147-150,
51. O'Brien WJ, Groh CL, Boenkc KM, Mora GP, Tien TY. The strengthing mechanism of a magnesia core ceramic. Dent Mater 1993:9: 242-245.
52. O'Brien WJ. Magnesia ceramic jacct crowns. Dent Clin North am 1985: 29:719-273.
53. Pcra P, Gİlodi S, Bass F. Carossa S in vitro marginal adaptation of alumina porcelain ceramic crowns. J Prosthet Dent 1994; 72(6): 585-590,
54. Phillips RW. Dental ceramics. Science of" denial materials. 9. Ed, W.B- Saunders Company, Philadelphia. 1991: 505-527.
55. Pröbstcr L, Diehl J. Slip-casting alumina ceramics for crown and bridge restorations. Quint Int. 1992; 23(1): 25-31.
56- l'röbsrer L, Kyrchner F. In vitro sticngth evaluation of a new ceramic restorative system. NOF/CED - Meeting Kol ding. Abst. Nr: 333, 1993.
57. Riley EJ. Ccrestore. Tylmann's theory and practice of fixed prosthodontics 8 ed. Ishiyaku Euro Amerika, İne, St. Louis, 1989: 435-446.
58. Sato T, Wohl wend A, Scharer P-'•Shrink-rree^ceramic crown system: Factors infkicncing Lhe core margin fit. Quint Dent Techno 1986; 10(2): 81-87,
59. Schaerer P, Sato T, Wohlwend A. A comparison of the marginal fit of three cast ceramic crown systems. J Prosthet Dent 1988; 59(5): 534-542.
60. Seghi RR. Denry 1, Brajcvic F. Effect of ion exchange on hardness and fracture toughness of dental ceramics. Int J Prosth 1992; 5(4): 309-314.
61. Seghi RR, Sorensen JA, Fngelman MJ, Torres TJ. Flexural strength of new ceramic materials. J Dent Rest. 1990; 69, Abst. No: 1521.299¬62. Scrlgö/. A, Gcmalmaz D. Al kumru H, Yoruç H.
Luting composite thickness of two ceramic inlay systems. J Prosth Rest Dent, 1995; 3(4): 151 -154.
63. -Sherd' MH. Jacobı R, Lindke F. The ceramic reverse three quarter crown for anterior teeth: Laboratory' procedures. J Prosthet Dent 1990; 64(2): 127-130.
64. Shillinburg EFT. Hobo S. Whit sett L. Porcelain restorations. Fundamentals of fixed prosthodontics. 2nd ed. Quint. Pub. Inc, Co, Chicago, 1981; 419-442.
65. Smith BGN. Types of crown. Planning and making crowns and bridges. 2nd ed.United kingdom, 1990: 22-37.
66. Sorensen JA, Avcra Si*. Fanuscu MI. Effect of veneer porcelain on all ceramic crown strength. J Detit Res, 1992; 71: Abstr. Nr. 1718.
67. Southan DF. I he porcelain jaket dental ceramics, Quint. Pub. Inc.. Co, Chicago. 1983: 207-230.
68. Sozio RB. Riley EJ- The shrink free ceramic crown. J Prosthet Dent 1983; 49(2): 182-187.
69. So/.io RB, Riley El. Shrink free ceramic. Dent Clin North Am 1985: 29(4): 705-717.
70. Strub JR. Vollkeratnische systems. Dtsch ZahnarztZ 1992; 47(9): 566-571.
71. Studcr S. I-ehner C, Scharer P. Glass ceramic inlays and onlays made by IPS Empress: First clinical rcsuk.JDent Res, 1992; 71: 658.
72. Sulik WD- The Dicor castable glass-ceramic sistem. Tylmann's theory and practice of fixed prosthodontics 8 cd. Ishiyaku Euro America, Inc, St. Louis. 1989:447-454.
73-Tuntupawon M, Wilson PR. The nd'ect of cement thickness on the fracture strength of all ceramic crowns. AustDentJ, 1995:40(1): 17-21.
74. Iltiterbrink G. Clinical aspects of full ceramic sistems. Ivoclar^Vivadent Report. Nr: 10, 1994: July 2I-3Ü
87
Atatürk Univ.Diş Hek.Fak Derg, Cilt: 10, Sayı:2, Sayfa:79-88,2000
Y ÜKSBL.ÇEKİÇ, ÖZKAN
75. Untcrbriıık G. IPS Empress, Ein neııes voli keramik osteins ZWR, 1991; lOOJahrg., NY. 10,-791.
76. Vahidi F, Egloff DT, Panno FV. Evaluation of marginal adaptation of all ceramic: crowns and mctaJ ceramic crowns. I Prosthet Dent 1991, 66(4): 426-43 1.
77. Wcbcr M, Chan CR, Gcis-Gcrstorfcr J, Simoni.s A. Kmipfer D. Procedural investigations and early clinical experiences with the full ceramic Ccrestojc crown system. Quint. Int. 1985; 7: 463-472.
78. Weaver JD, Johnson Gil, Bales DJ. Marginal adaptation of castable ceramic crowns. J Prosthet Dent 1991; 66(G): 746-753.
79. Wohlewend A, Slruh JR. Scharer P, Metal ceramic and all porcelain restorations: Current considerations, ini j Prosth 1989; 2(1): 13-26.
80. Wohlwcnd A, Brodbcck Lf. Das IPS Empress Keramikimay fionderdruck aus "Innuviitionen i'iir die Zahnheikmde" liir Ivoclar AG. Henderslro He 2. FL. 9494 Schaan/'Liechtetein,
SI. Wohhveiid A, Scharer P. The Empress technipite. A new technique for the fabrication of full ceramic crowns, inlays and veneers. Quint Zahnlcchnik 1990: 16:966-978.
82. Yamamolo M. Factors affecting the strength of metal ceramics. Metal ceramics principles and method of Makato Yamamolo. Quinles f'uh. Co., Inc. Chicago, 1985: Chapter Î
83. Yiiftset G.
Tekrarlana
n fırınlama işlemlerinin ii'S Empress sistem ile hazırlanan kronların kenar uyumuna etkisi. Doktora Tezi, H.Ü, Sağlık Bilimleri Enstitüsü, Ankara, 1996.
84.
Zaimoğl
u A. Can G, Ersoy E, Aksu L. Dental porselenler. Dışhekimliğinde Maddeler Bilgisi, Ankara. AÜ Diş llek. Fak. Derg. Yayınlarından, 1993: 355-390.