DENTİN BAĞLAYICI SİSTEMLERİN BAĞLANMA DAYANIKLILIĞINI DEĞERLENDİRME YÖNTEMLERİ

Evaluation of Bonding Durability of Dentin Bonding Systems

Journal Name:

Publication Year:

Abstract (2. Language): 
Over the last decade, the classic concept of three-step bonding to dental tissues has developed rapidly to more user-friendly, simplified adhesive systems. These comprise the two-step total etch and the two step self-etch systems. The latter, initially avaible in two steps, were further reduced to a one step procedure for simpler and faster application. However, despite the user-friendly features of this category of adhesives, bring about a certain disadvantage. The gold standart for evaluating the performance of dental materials are the controlled clinical trial. The constand, rapid evolution of adhesive materials increases the number of long-term clinical trials needed. However, due to increasing costs and the immediate demand for information, there is a need for surrogate methods. The establishment of an in vitro methodology capable of reproducing some in vivo challenges is crucial for better understanding of restorative materials behavior. The use of some methodologies in laboratory studies of dental materials has been considered potantial methods to simulate in vivo challenges. The aim of this study was to review the mechanism of the durability of adhesive interface, the in vitro aging methods in order to simulate the bonding degradation that occurred in the oral environment and the current information and research on dentin adhesives durability.
Abstract (Original Language): 
Son yıllarda 3 aşamalı total etch sistemler hızla geliştirilerek yerini uygulama aşamaları daha kolay olan 2 aşamalı total etch ve 2 aşamalı self etch sistemlere bırakmıştır. İki aşamalı sistemlerden sonra uygulama aşamaları basitleştirilmiş olan tek aşamalı sistemler geliştirilmiştir. Uygulama aşamaları basit olmasına karşın bu sistemler bir takım dezavantajları da beraberinde getirmektedir. Klinik uygulamalarda sıklıkla kullanılan bu materyallerin performanslarını incelemenin en etkin yolu ise klinik deneylerdir. Adeziv sistem teknolojisindeki hızlı gelişmeler daha fazla sayıda klinik deney ihtiyacını doğurmuştur. Ancak klinik deneylerin yüksek maliyetlerde olması, uzun zaman alması ve materyallerdeki hızlı değişim klinik deneylere alternatif yeni araştırma metotlarının ihtiyacını beraberinde getirmiştir. İn vivo ortamda restoratif materyallerin maruz kaldıkları durumları taklit etmek amacıyla bir takım in vitro metodolojiler geliştirilmiştir. Bu makalenin amacı, restorasyon ara yüzeyinde oluşturulan bağlanmanın yıkılma mekanizması, ağız ortamında meydana gelen bağlanma yıkımını taklit etmek amacıyla oluşturulan in vitro yaşlandırma yöntemleri ve dentin adezivlerin bağlanma dayanıklılığı ile ilgili güncel bilgi ve araştırmaları derlemektir.
73
91

REFERENCES

References: 

1. Shirai K, Munck JD, Yoshida Y, Inoue
S, Lambrechts P, Suziki K, Shintani H,
Meerbeek BV. Effect of cavity configuration
and aging on the bonding effectiveness of
six adhesives to dentin. Dent Mater, 2005;
21: 110-24.
2. De Munck JD, Landuyt KV, Peumans
M,Poitevin A, Lambrechts P, Braem M,
Meerbeek BV. A critical review of durability
of adhesion to tooth tissue: methods and
results. J Dent Res, 2005; 84(2):118-32.
3. Tay FR, Pashley DH. Have dentin adhesives
become too hydrophilic? J Can Dent
Assoc, 2003; 69: 726-31.
4. Hashimoto M, Ohno H, Kaga M, Endo
K, Sano H, Oguchi H. In vivo degradation
of resin-dentin bonds in humans over 1 to 3
years. J Dent Res, 2000; 79: 1385-91.
5. Amaral FLB, Colucci V, Palma-Dibb
RG, Corona Silmara AM. Assessment of
in vitro methods used to promote adhesive
interface degradation: a critical review. J
Esthet Restor Dent, 2007; 19: 340-54.
6. Gale MS, Darvell BW. Thermal cycling
procedures for laboratory testing of dental
restorations. J Dent, 1999; 27: 89-99.
7. De Munck JD, Van Meerbeek B, Van
Landuyt K, Lambrechts P. Influence of a
shock absorbing layer on the fatigue resistance
of a dentin-biomaterial interface. Eur
J Oral Sci, 2005; 113: 1-6.
8. Sano H. Microtensile testing, nanoleakage,
and biodegradation of resin-dentin
bonds. J Dent Rest, 2006; 85(1): 11-14.
9. Reis A, Carrilho MRO, Ghaneme E,
Pereira PNR, Giannini M, Nikaido T, Tagami
J. Effects of water-storage on the physical
and ultramorphological features of adhesives
and primer/adhesive mixtures. Dent Mater
J, 2010; 29(6): 697-705.
10. Breschi L, Mazzoni A, Ruggeri A,
Cadenaro M, Di Lenarda R, Dorigo EDS.
Dental adhesion review: aging and stability
of the bonded interface. Dent Mater, 2008;
24: 90-101.
11. Hashimoto M, Ohno H, Sano H, Kaga
M, Oguchi H. In vitro degradation of resindentin
bonds analyzed by microtensile bond
test, scanning and transmission electron microscopy.
Biomaterials, 2003; 24: 3795-803.
12. Vaidyanathan TK, Vaidyanathan J.
Review Recent Advances in the theory and
mechanism of adhesive resin bonding to dentin:
a critical review. Appl Biomater, 2009;
88B: 558-78.
13. Giannini M, Arrais CAG, Vermelho
PM, Reis RS, Santos LPS, Leite ER. Effects
of the solvent evaporation technique on the
degree of conversion of one-bottle adhesive
systems. Oper Dent, 2008; 33(2): 149-54.
14. Okada T, Ikada Y. In vitro and in vivo
digestion of collagen covalently immobilized
onto the silicone surface. J Biomed Mater
Res, 1992; 26: 1569-81.
15. Soderholm KJ, Richards ND. Wear
resistance of composites: a solved problem?
Gen Dent, 1998; 46: 256-63.
16. Pashley DH, Tay FR, Yiu C, Hashimoto
M, Breschi L, Carvalho RM, Itı S.
Collagen degradation by host-derived enzymes
during aging. J Dent Res, 2004; 83(3):
216-21.
17. Marshall SJ, Bayne SC, Baier R, Tomsia
AP, Marshall GW. A review of adhesion
N. Tekçe, M. Demirci, S. Tuncer
87
science. Dent Mater, 2010; 26: 11-16.
18. Hashimoto M. A review- Micromorphological
evidence of degradation in resin-
dentin bonds and potential preventional
solutions. Appl Biomater, 2010; 92: 268-80.
19. Tay FR, Pashley DH, Suh BI, Hiraishi
N, Yiu CK. Buonocore memorial lecture.
Water treeing in simplified dentin adhesivesdeja
vu? Oper Dent, 2005; 30: 561-79.
20. Yiu CKY, King NM, Pashley DH,
Suc BI, Carvalho RM, Carrilho MRO, Tay
FR. Effect of resin hydrophilicity and water
storage on resin strength. Biomaterials, 2004;
25: 5789-96.
21. Torkabadi S, Nakajima M, Ikeda M,
Foxton RM, Tagami J. Influence of bonded
enamel margins on dentin bonding stability
of one-step self-etching adhesives. J Adhes
Dent, 2009; 11: 347-53.
22. Hashimoto M, Fujita S, Kaga M,
Yawaka Y. In vitro durability of one-bottle
resin adhesives bonded to dentin. Dent Mater
J, 2007; 26(5): 677-86.
23. Hosaka K, Nakajima M, Takahashi
M, Itoh S, Ikeda M, Tagami J, Pashley DH.
Relationship between mechanical properties
of one-step self-etch adhesives and water
sorption. Dent Mater, 2010; 26: 360-67.
24. Ito S, Hashimoto M, Wadgaonkar B,
Svizero N, Carvalho RM, Yiu C. Effects of
resin hydrophilicity on water sorption and
changes in modulus of elasticity. Biomaterials,
2005; 26: 6449-59.
25. Tay FR, Pashley DH, Suh BI, Carvalho
RM, Itthagarun A. Single-step adhesives
are permeable membranes. J Dent, 2002;
30: 371-82.
26. Tay FR, Pashley DH. Water treeing
– a potential mechanism for degradation of
dentin adhesives. Am J Dent, 2003; 16: 6-12.
27. Toledano M, Osorio R, Osorio E, Aguilera
FS, Yamauti M, Pashley DH, Tay FR.
Durability of resin-dentin bonds: effects of
direct/indirect exposure and storage media.
Dent Mater, 2007; 23: 885-92.
28. Meerbeek BV, Peumans M, Poitevin
A, Mine A, Ende AV, Neves A, Munck JD.
Relationship between bond strength tests
and clinical outcomes. Dent Mater, 2010;
26: 100-21.
29. Ohno H, Araki Y, Endo K, Yamane Y,
Kawasahima I. Evaluation of water durability
at adhesion ınterfaces by peeling test of
resin film. Dent Mater J, 1996; 15(2): 183-92.
30. Cenci MS, Venturini D, Cenci TP,
Piva E, Demarco FF. The effect of polishing
techniques and time on the surface characteristics
and sealing ability of resin composite
restorations after one-year storage. Oper
Dent, 2008; 33: 169-76.
31. Fukushima T, Inoue Y, Miyazaki K, Itoh
T. Effect of primers containing N methylolacrylamide
or N-methylolmethacrylamide
on dentin bond durability of a resin composite
after 5 years. J Dent, 2001; 29: 227-34.
32. De Munck J, Van Meerbeek B, Yoshida
Y, Inoue S, Vargas M, Suzuki K. Four-year
water degradation of total-etch adhesives
bonded to dentin. J Dent Res, 2003; 82: 136-
40.
33. Ferracane JL, Berge HX, Condon JR.
In vitro aging of dental composites in watereffect
of degree of conversion, filler volume,
and filler/matrix coupling. J Biomed Mater
Res, 1998; 42: 465-72.
34. Santerre JP, Shajii L, Leung BW. Relation
of dental composite formulations to their
degradation and the release of hydrolyzed
polymeric-resin-derived products. Crit Rev
Oral Biol Med, 2001; 12: 136-51.
35. Burrow MF, Satoh M, Tagami J. Dentin
bond durability after three years using
a dentin bonding agent with and without
priming. Dent Mater, 1996; 12: 302-307.
36. Armstrong SR, Keller JC, Boyer DB.
Mode of failure in the dentinadhesive resinDentin
Bağlayıcı Sistemlerin Bağlanma Dayanıklılığını Değerlendirme Yöntemleri
88
resin composite bonded joint as determined
by strengthbased (μTBS) and fracture-based
(CNSB) mechanical testing. Dent Mater,
2001; 17: 201-10.
37. Shono Y, Terashita M, Shimada J,
Kozono Y, Carvalho RM, Russell CM. Durability
of resin-dentin bonds. J Adhes Dent,
1999; 1: 211-18.
38. Kitasako Y, Burrow MF, Nikaido T,
Tagami J. The influence of storage solution
on dentin bond durability of resin cement.
Dent Mater, 2000; 16: 1-6.
39. Finer Y, Santerre JP. Salivary esterase
activity and its association with the biodegradation
of dental composites. J Dent Res,
2004; 83: 22-26.
40. Frankenberger R, Krämer N, Petschelt
A. Long-term effect of dentin primers on
enamel bond strength and marginal adaptation.
Oper Dent, 2000; 25: 11-19.
41. Armstrong SR, Keller JC, Boyer DB.
The influence of water storage and C-factor
on the dentin-resin composite microtensile
bond strength and debonded pathway utilizing
a filled and unfilled adhesive resin. Dent
Mater, 2001; 17: 268-76.
42. Nunes TG, Ceballos L, Ososrio R,
Toledano M. Spatially-resolved photopolymerization
kinetics and oxygen inhibition
in dntal adhesives. Biomaterials, 2005; 26:
1809-17.
43. De Munck J, Mine A, Poitevin A,
Van Ende A, Cardoso MV, Van Landuyt KL.
Meta-analytical review of parameters involved
in dentin bonding. J Dent Res, 2012;
91: 351-57.
44. Leloup G, D’Hoore W, Bouter D,
Degrange M, Vreven J. Meta-analytical review
of factors involved in dentin adherence.
J Dent Res, 2001; 80: 1605-14.
45. Tjaderhane L, Nascimento FD, Breschi
L, Mazzoni A, Tersariol IL, Geraldeli S,
Tezvergil-Mutluay A, Carrilho MR, Carvalho
RM, Tay FR, Pashley DH. Optimizing
dentin bond durability: control of collogen
degradation by matrix metalloproteinases
and cysteine cathepsins. Dent Mater, 2013;
29(1): 116-35.
46. Reis A, Loguercio AD, Carvalho RM,
Grande RHM. Durability of resin dentin
interfaces: effets of surface moisture and
adhesive solvent component. Dent Mater,
2004; 20: 669-76.
47. Hashimoto M, Fujita S, Kaga M, Yawaka
Y. Effect of water on bonding of onebottle
self-etching adhesives. Dent Mater J,
2008; 27(2): 172-78.
48. Hashimoto M, Ohno H, Sano H, Tay
FR, Kaga M, Kudou Y, Oguchi H, Araki Y,
Kubato M. Micromorphological changes in
resin-dentin bonds after 1 year water storage.
J Biomed Mater Res, 2002; 63: 306-11.
49. Gamborgi GP, Loguercio AD, Reis A.
Influence of enamel border and regional variability
on durability of resin-dentin bonds.
J Dent, 2007; 35: 371-76.
50. Heitze SD. Clinical relevance of tests
on bond strength, microleakage and marginal
adaptation. Dent Mater, 2013; 29(1): 59-84.
51. Hashimoto M, Fujita S, Nagano F,
Ohno H, Endo K. Ten-years degradation of
resin-dentin bonds. Eur J Oral Sci, 2010;
118: 404-10.
52. Reis A, Grandi V, Carlotto L, Bortoli
G, Patzlaff R, Lourdes M, Loguercio AD.
Effect of smear layer thicness and acidity
of self-etching solitions on erly and long
term bond strength to dentin. J Dent, 2005;
33: 549-59.
53. Paul SJ, Leach M, Rueggerberg FA,
Pashley DH. Effect of water content on the
physical properties of model dentin primer
and bonding resins. J Dent, 1999; 27: 209-14.
54. Sadek FT, Goracci C, Cardoso PEC,
Tay FR, Ferrari M. Microtensile bond
strength of current dentin adhesives meaN.
Tekçe, M. Demirci, S. Tuncer
89
sured immediately and 24 hours after application.
J Adhes Dent, 2005; 7: 297-302.
55. Reis A, Cardoso P, Vieira L, Baratieri
L, Grande R, Loguercio AD. Effect of prolonged
application times on the durability
of resin-dentin bonds. Dent Mater, 2008;
24: 639-44.
56. Toledano M, Proença JP, Erhardt
MCG, Osorio E, Aguilera FS, Osorio R,
Tay FR. Increases in dentin-bond strength
if doubling application time of an acetonecontaining
one step adhesive. Oper Dent,
2007; 32(2): 133-37.
57. Cardoso Pde C, Loguercio AD, Vieira
LC, Baratieri LN, Reis A. Effect of prolonged
application times on resin-dentin bond
strengths. J Adhes Dent, 2005; 7: 143-49.
58. Sano H, Yoshikawa T, Pereira PN, Kanemura
N, Morigami M, Tagami J, Pashley
DH. Long-term durability of dentin bonds
made with a self etching primer, in vivo. J
Dent Res, 1999; 78(4): 906-11.
59. Mitsui FHO, Peris AR, Caavalcanti
AN, Marchi GM, Pimenta LAF. Influence
of thermal and mechanical load cycling on
microtensile bond strenhths of total and selfetching
adhesive systems. Oper Dent, 2006;
31(2): 240-47.
60. Miyazaki M, Sato M, Onose H, Moore
BK. Influence of thermal cycling on dentin
bond strength of two-step bonding systems.
Am J Dent, 1998; 11: 118-22.
61. Amano S, Yamamoto A, Tsubota K,
Rikuta A, Miyazaki M, Platt JA, Moore BK.
Influence of thermal and mechanical load
cycling on the microtensile bond strength
of self- etching adhesives. Oper Dent, 2006;
31: 616-22.
62. Li H, Burrow MF, Tyas MJ. The effect
of thermocycling regimens on the nanoleakage
of dentin bonding systems. Dent Mater,
2002; 18: 189-96.
63. Santos PA, Garcia PPNS, Palma-
Dibb RG. Shear bond strength of adhesive
systems-effects of primer and thermocycling.
Pesqui Odontol Bras, 2002; 16: 37-42.
64. Nikaido T, Kunzelmann KH, Chen H.
Evaluation of thermal cycling and mechanical
loading on bond strength of a self-etching
primer system to dentin. Dent Mater, 2002;
18: 269-75.
65. Bastioli C, Romano G, Migliaresi C.
Water sorption and mechanical properties
of composites. Biomaterials, 1990; 11(3):
219-23.
66. Yang B, Adlung R, Ludwig K, Böbmann
K, Pashley DH, Kern M. Effect o
structural change o collagen fibrils on the
durability o dentin bonding. Biomaterials,
2005; 26: 5021-31.
67. Rosales-Leal JI. Microleakage of class
V composite restorations placed with etch
and rinse and self etching adhesives before
and after thermocycling. J Adhes Dent, 2007;
9: 255-59.
68. Dos Santos PA, Garcia PP, Palma-
Dibb RG. Shear bond strength of adhesive
systems to enamel and dentin. Thermocycling
influence. J Mater Med, 2005; 16(8):
727-32.
69. Schuckar M, Geurtsen W. Proximocercival
adaptation of class II-composite
restorations after thermocycling: a quantitative
and qualitative study. J Oral Rehabil,
1997; 24: 766-75.
70. Mjör IA, Shen C, Eliasson ST. Placement
and replacement of restorations in
general dental proctice. Oper Dent, 2002;
27: 117-23.
71. Salz U, Zimmermman J, Zeuner F,
Moszner N. Hydrolitic stability of selfetching
adhesive systems. J Adhes Dent,
2005; 7: 107-16.
72. Blunck U, Zaslansky P. Effectiveness
of all in one adhesive systems tested
by thermocycling fallowing short and long
Dentin Bağlayıcı Sistemlerin Bağlanma Dayanıklılığını Değerlendirme Yöntemleri
90
term water storage. J Adhes Dent, 2007; 9:
231-40.
73. Lodovici E, Reis A, Geraldeli S, Ferracane
JL, Ballester RY, Filho LER. Does
adhesive thickness affect resin-dentin bond
strength after thermal/load cycling? Oper
Dent, 2009; 34(1): 58-64.
74. Bates JF, Stafford GD, Harrison A.
Masticatory function –a review of the literature
(II). Speed of the movement of the mandible,
rate of chewing and forces developed
in chewing. J Oral Rehabil, 1975; 2: 349-61.
75. Frakenberger R, Tay FR. Self-etchand-
rinse adhesives: effect of thermomechanical
fatigue loading on marginal quality
of bonded resin composite restorations. Dent
Mater, 2005; 21: 397-412.
76. Abdalla AI, El Zohairy AA, Aboushelib
MMN, Feilzer AJ. Influence of thermal
and mechanical load cycling on the microtensile
bond strength of self- etching adhesives.
Am J Dent, 2007; 20: 250-54.
77. Monticelli F, Osorio R, Proença JP,
Toledano M. Resistance to degradation of
resin-dentin bonds using a one-step HEMAfree
adhesive. J Dent, 2007; 35: 181-86.
78. Toledano M, Osorio R, Albaladejo
A, Aguilera FS, Osorio E. Differential effect
of in vitro degradation on resin-dentin
bonds produced by self-etch versus total-etch
adhesives. J Biomed Mater Res A, 2006;
77(1): 128-35.
79. Bedran De Castro AK, Pereira PN,
Pimenta LA, Thompson JY. Effect of thermal
and mechanical load cycling on nanoleakage
of class II restorations. J Adhes Dent, 2004;
6: 221-26.
80. Li H, Burrow MF, Tyas MJ. The effect
of loading cycling on the nanoleakage of
dentin bonding systems. Dent Mater, 2002;
18: 111-19.
81. Nikaido T, Kunzelmann KH, Ogata
M, Harada N, Yamaguchi S, Cox CF, Hickel
R, Tagami J. The in vitro bond strengths of
two adhesive systems in class I cavities of
human molars. J Adhes Dent, 2002; 4(1):
31-39.
82. Bedran-De-Castro AK, Pereira PN,
Pimenta LA. Long term bond strength of
restorations subjected to thermo-mechanical
stresses over time. Am J Dent, 2004; 17(5):
337-41.
83. Yamauti M, Hashimoto M, Sano H,
Ohno H, Carvalho RM, Kaga M. Degradation
of resin-dentin bonds using NaOCl
storage. Dent Mater, 2003; 19: 399-405.
84. De Munck J, Ermis RB, Koshiro
K, Inoue S, Ikeda T, Sano H, Van Landuyt
KL, Meerbeek BV. NaOCI degradation of a
HEMA-free all-in-one adhesive bonded to
enamel and dentin following two air-blowing
techniques. J Dent, 2007; 35(1): 74-83.
85. Sacramento PA, Carvalho FBD, Pascon
FM, Borges AFS, Alves MC, Hosoya
Y, Rontani RMP. Influence of NaOCI Irrigation
and water storage on the degradation
and microstructure of resin/primary dentin
interface. J Adhes Dent, 2011; 13: 213-20.
86. Toledano M, Perdigao J, Osorio R,
Osorio E. Effect of dentin deproteinization
on microleakage of class V composite restorations.
Oper Dent, 2000; 25: 497-504.
87. Sakae T, Mishima H, Kozawa Y.
Changes in bovine dentin mineral with sodium
hypochlorite treatment. J Dent Res,
1988; 67(9): 1229-34.
88. Featherstone JDB, O’Really MM,
Shariati M, Brugler S. Enhancement of remineralization
in vitro and in vivo. In Leach AS
editor. Factors relating to demineralization
and remineralization of the teeth. Oxford
(English): IRL, 1986. p. 23-34.
89. Turssi CP, Hara AT, Serra MC, Rodrigues
AL. Effect of storage media upon the
surface micromorphology of resin-based restorative
materials. J Oral Rehabil, 2002; 29:
N. Tekçe, M. Demirci, S. Tuncer
91
864-71.
90. Hashimoto M, Tay FR, Ohno H, Sano
H, Kaga M, Yiu C, Kumagai H, Kudou Y,
Kubota M, Oguchi H. SEM and TEM analysis
of water degradation of human dentinal
collagen. J Biomed Mater Res: Part B, Appl
Biomater 2003; 66(1): 287-98.
91. Tjaderhane L, Larjava H, Sorsa T,
Uitto VJ, Larmas M, Salo T. The activation
and function of host matrix metalloproteinases
in dentin matrix breakdown in caries
lesions. J Dent Res, 1998; 77(8): 1622-29.
92. Tjaderhane L, Sulkala M, Sorsa T,
Teronen O, Larmas M, Salo T. The effect
of MMP inhibitor metastat on fissure caries
progression in rats. Ann NY Acad Sci, 1999;
878: 686-88.
93. Sulkala M, Wahlgren J, Larmas M,
Sorsa T, Teronen O, Salo T, Tjüderhane L.
The effects of MMP inhibitors on human
salivary MMP activity and caries progression
in rats. J Dent Res, 2001; 80(6): 1545-49.
94. Tezvergil-Mutluay A, Agee KA, Hoshika
T, Carrilho M, Breschi L, Tjaderhane
L. The requirement of zinc and calcium ions
for functional MMP activity in demineralized
dentin matrices. Dent Mater, 2010; 26:
1059-67.
95. Tezvergil-Mutluay A, Agee KA, Hoshika
T, Tay FR, Pashley DH. The inhibitory
effect of polyvinylphosphonic acid on functional
matrix metalloproteinase activities in
human demineralized dentin. Acta Biomater,
2010; 6(10): 4136-42.
96. Tezvergil-Mutluay A, Mutluay MM,
Agee KA, Seseogullari-Dirihan R, Hoshika
T, Cadenaro M. Carbodiimide cross-linking
inactivates soluble and matrix-bound MMPs,
in vitro. J Dent Res, 2012; 91: 192-96.
97. Salz U, Bock T. Testing adhesion of
direct restoratives to dental hard tissue: a
review. J Adhes Dent, 2010; 12: 343-71.

Thank you for copying data from http://www.arastirmax.com